Strategies For Handling Plastic Bottle Waste In Gorontalo City Through The Utilization Of Asphalt Concrete Wearing Course (AC-WC) Additives

Fidya Mayestika, Universitas Negeri Gorontalo, Indonesia
Sukirman Rahim, Universitas Negeri Gorontalo, Indonesia
Fitriyane Lihawa, Universitas Negeri Gorontalo, Indonesia
Ramli Utina, Universitas Negeri Gorontalo, Indonesia
Marike Machmud, Universitas Negeri Gorontalo, Indonesia

Abstract


The amount of plastic waste, especially disposable plastic bottle waste (PET), needs to be utilized. plastic bottle waste is a flexible material that can be used as an alternative additive to the pavement mixture so as to reduce the production of PET disposable bottle waste. So this research needs to be done to find out its utilization. The purpose of this research is to analyze Polyethylen Terephtalate (PET) plastic bottle waste can be used as an additive and analyze the amount of Polyethylen Terephtalate (PET) bottles needed for Asphalt Concrete Wearing Course (AC-WC) pavement mixtures. The method used is an experimental method carried out in two stages. The first stage of Marshall testing without using plastic to find the Optimum Asphalt Content (KAO) with variations of 4%, 4.5%, 5%, 5.5%, 6%, 6.5%. The second stage of Marshall testing using the optimum asphalt content (KAO) obtained from stage one with additional variations of Polyethylen Terephtalate (PET) plastic bottle waste 1%, 2%, 3%, 4%, 5% to get the optimum PET content. The results of stage one Marshall testing obtained an optimum asphalt content of 5.675%, while Marshall in the second stage obtained an optimum PET content of 0.45% equivalent to 0.0026 gr and all types of Marshall parameters met the Bina Marga 2018 revision 2 specifications for mixing Asphalt Concrete Wearning Course (AC-WC). Each production of one ton of Asphalt Concrete Wearning Course (AC-WC) requires 204.3 bottles of Polyethylen Terephtalate (PET) plastic.

The amount of plastic waste, especially disposable plastic bottle waste (PET), needs to be utilized. plastic bottle waste is a flexible material that can be used as an alternative additive to the pavement mixture so as to reduce the production of PET disposable bottle waste. So this research needs to be done to find out its utilization. The purpose of this research is to analyze Polyethylen Terephtalate (PET) plastic bottle waste can be used as an additive and analyze the amount of Polyethylen Terephtalate (PET) bottles needed for Asphalt Concrete Wearing Course (AC-WC) pavement mixtures. The method used is an experimental method carried out in two stages. The first stage of Marshall testing without using plastic to find the Optimum Asphalt Content (KAO) with variations of 4%, 4.5%, 5%, 5.5%, 6%, 6.5%. The second stage of Marshall testing using the optimum asphalt content (KAO) obtained from stage one with additional variations of Polyethylen Terephtalate (PET) plastic bottle waste 1%, 2%, 3%, 4%, 5% to get the optimum PET content. The results of stage one Marshall testing obtained an optimum asphalt content of 5.675%, while Marshall in the second stage obtained an optimum PET content of 0.45% equivalent to 0, 0026 gr and all types of Marshall parameters met the Bina Marga 2018 revision 2 specifications for mixing Asphalt Concrete Wearning Course (AC-WC). Each production of one ton of Asphalt Concrete Wearning Course (AC-WC) requires 204.3 bottles of Polyethylen Terephtalate (PET) plastic.


Full Text:

PDF


DOI: https://doi.org/10.21831/ijoce.v7i1.67871

Refbacks

  • There are currently no refbacks.


Our journal is indexed by:

    

Creative Commons License 

This work is licensed under a Creative Commons Attribution-NonCommercial-NoDerivatives 4.0 International License.

Indonesian Journal of Chemistry and Environment (IJoCE)

e-ISSN 2599-3186
Published by: Department of Chemistry, Universitas Negeri Yogyakarta

 

View My Stats